Continuing my cladding series…
Unfortunately, the negative holder doesn´t allow a full-frame scan, so the pipe on the left is slightly cut off.
This is one of my first self-developed negatives. XTOL 1+1 11:30min @20°C (agitating for the first 30s, then 5s every 30 seconds using Jobo 2520 with 2509n, 4 sheets), citric acid stop bath, Moersch ATS Schnellfixierbad alkalisch 1+4 for 6 minutes.